Reinforcing Steel Bars
Timber
Wooden Floors
Tiles
Deck
Roof Tiles
Glass Blocks
Grouting / Adhesives / Rendering Mortars
Raised Floors
Riwega
Isover
Plywood
Hardboard/Softboard
Osb
Mdf/Mdf Veneer
ChipBoard/Wood Veneered Chipboard/Melamine
Wooden Facades
Gypsum Boards
Reinforcing Steel Bars
Timber
Wooden Floors
Tiles
Deck
Roof Tiles
Glass Blocks
Grouting / Adhesives / Rendering Mortars
Raised Floors
Riwega
Isover
Wooden Facades
Gypsum Boards
Home > Mdf/Mdf Veneer

Mdf/Mdf Veneer

Medium-density fiberboard (MDF or MDFB) is an engineered wood product formed by breaking down softwood into wood fibres, often in a defibrator, combining it with wax and resin, and forming panels by applying high temperature and pressure. It is a building material similar in application to plywood but made up of separated fibres, not wood veneers. It is denser than normal particle board.

Large-scale production of MDF began in the 1980s. Its name derives from the distinction in densities of fiberboard. MDF typically has a density of 600-800 kg/m³, in contrast to particle board (160-450 kg/m³) and to high-density fiberboard (500-1450 kg/m³). Similar manufacturing processes are used in making all types of fiberboard.

MDF is also known as Custom wood or Craft wood.

MDF has been controversial in regard to its use of formaldehyde resins and the associated health risks. Thus, other resins are being considered and used instead of formaldehyde.

Manufacturing:

MDF is a wood product created by breaking down softwood into a powder, which is then mixed with wax and resin. The final finish is created by submitting the boards to high pressure and temperatures.

In Australia the main species of tree used for MDF is plantation-grown radiate pine. However a variety of other products have also been used including other woods, waste paper and fibers.

The trees are debarked after being cut. The bark can be sold for use in landscaping, or burned in on-site furnaces. The debarked logs are sent to the MDF plant where they go though the chipping process. A typical disk chipper contains 4-16 blades. Any resulting chips that are too large may be re-chipped; undersized chips may be used as fuel. All chips are then washed and checked for defects.

The chips are then compacted using a screw feeder, and will be heated for 30-120 seconds to soften the wood; they are then fed into a defibrator which maintains high pressure and temperature. The pulp that exits from the defibrator is fine, fluffy, and light in weight and in colour.

From the defibrator the pulp enters a blow line where it is joined with wax (to improve moisture resistance) and resin (to stop the pulp from forming bundles). The material expands in size and is then heated by heating coils. When it comes out it may be stored in bins for an indefinite length of time.

After this drying period the board goes through a "Pendistor" process which creates 230-610 mm thick boards. Then it is cut and continues to the press. Here it is pressed for a few minutes, to make a stronger and denser board.

After pressing MDF is cooled in a star dryer, trimmed and sanded. In certain applications boards are also laminated for extra strength.

The Environmental Impact of MDF has greatly improved over the years. Today many MDF boards are made from a variety of materials. These include other woods, scrap, recycled paper, bamboo, carbon fibers and polymers, steel, glass, forest thinning and sawmill off-cuts.